Title: Structural characterization of highly cis-1,4-polybutadiene: A comparing study in swollen and solid state using NMR technique
Authors: Jitladda Sakdapipanich
Tippawan Kowitteerawut
Kawahara Seiichi
Yasuyuki Tanaka
Mahidol University
Nagaoka University of Technology
Keywords: Chemistry;Materials Science;Physics and Astronomy
Issue Date: 31-Aug-2001
Citation: Polymer Bulletin. Vol.46, No.6 (2001), 479-485
Abstract: Commercial highly cis-1,4-polybutadiene was cured out by benzoyl peroxide from 3 to 12 phr in toluene solution. The structural characterization of resulting gel fraction or cured rubber was carried out in both swollen- and solid-state 13C-NMR measurements. The assignment of observed chemical shift proposed by using a shift factor method and empirical calculation using HOSE method.
URI: https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=0034886830&origin=inward
http://repository.li.mahidol.ac.th/dspace/handle/123456789/26504
ISSN: 01700839
Appears in Collections:Scopus 2001-2005

Files in This Item:
There are no files associated with this item.


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.