    ItemMetadata only
    Changes of retention unit and keeper-surface structure of neodymium-iron-boron magnetic attachments upon immersion in lactic acid, acetic acid, and artificial saliva
    (Mahidol University. Mahidol University Library and Knowledge Center, 2005) Trinuch Eiampongpaiboon; Jurai Nakaparksin
  • No Thumbnail Available
    PublicationMetadata only
    Effect of piper betle extract on anti-candidal activity, gelation time, and surface hardness of a short-term soft lining material
    (2020-01-01) Juthatip Kumpanich; Trinuch Eiampongpaiboon; Widchaya Kanchanavasita; Somsak Chitmongkolsuk; Jindaporn Puripattanavong; Mahidol University; Prince of Songkla University
    © 2020, Japanese Society for Dental Materials and Devices. All rights reserved. The purpose of this study was to evaluate anti-candidal activity, gelation time, and surface hardness of a short-term soft lining material incorporated with varying concentrations of Piper betle extract (0.25 to 20% w/w). Agar-diffusion assay was conducted to evaluate an inhibitory effect against Candida albicans. The gelation time was assessed and surface hardness was measured at 2 h and 7 days by Shore AO durometer. A soft liner containing at least 5% w/w of P. betle extract was observed the inhibitory effect against C. albicans. An increasing of P. betle concentrations provided larger inhibition zone. Incorporating 5% w/w of P. betle extract into the soft liner did not significantly alter its gelation time and surface hardness (ANOVA; p>0.05). The optimum composition at 5% w/w of P. betle extract can be used as an additive in the soft liner to provide the anti-candidal activity without significantly affect these two main properties.
  • Thumbnail Image
    PublicationOpen Access
    The effect of thickness on the contrast ratio and color of veneering ceramics.
    (2014-05) Phira Sithiamnuai; พีระ สิทธิอำนวย; Trinuch Eiampongpaiboon; ตรีนุช เอี่ยมพงษ์ไพบูลย์; Shrestha, Arati; Kallaya Suputtamongkol; กัลยา ศุพุทธมงคล; Kallaya Suputtamongkol; กัลยา ศุพุทธมงคล; Mahidol University. Faculty of Dentistry. Department of Prosthodontics
    Objectives: The objectives of this study were to evaluate the effect of thickness on the contrast ratio and color of two veneering ceramics. Materials and methods: Square shaped specimens (15mm x15 mm) were prepared from A3 shade of Vita VM9 (V) and IPS e-max Ceram (E) at four different thicknesses i.e., 0.6mm,0.8mm,1.2mm,1.5mm (n=5). All specimens were finished flat on a milling machine to the required dimension using 100 µ m diamond coated disc. The contrast ratio (CR= Yb / Yw ) and color difference (∆ E= [(L*1 -L2 *)2 + (a*1 - a*2 ) 2 + (b*1 -b*2 )]2 ) 1/2 were measured with a spectrophotometer and calculated. The statistical analyses for the mean contrast ratio (CR) of all groups were performed by two-way ANOVA and Tukey multiple comparison test at α=0.05. Color differences (∆E*) were compared between different thicknesses for the same brand and between different brands at the same thicknesses. Results: The results showed that the mean CR increased significantly with the increase in thickness from 0.6 to 1.5mm for both veneering ceramics; the CR of V 0.6 (0.61±0.01) was the lowest whereas CR of V 1.5 (0.87±0.00) and E 1.5 (0.87±0.01) were the highest. The brands did not significantly influence the mean contrast ratio in each thickness of veneering ceramics. For both veneering ceramics, a decrease in L*and an increase in a*were observed when the thickness increased. No influence of increasing thickness on b*was observed. Conclusions: The contrast ratio of two veneering ceramics was significantly influenced by thickness irrespective of the brands. L* and a* were influenced by thickness but not b*. When the thickness of the veneering ceramic was increased in both the brands, color changes were observed as an increase in ∆E* value.
  • No Thumbnail Available
    PublicationMetadata only
    Reactions: Antibacterial and bioactive dental restorative materials: Do they really work?
    (2018-11-15) Daniel Cn Chan; Wenjie Hu; Kwok Hung Chung; Robert Larsen; Steven Jensen; Densen Cao; Laura Gaviria; Joo L. Ong; Kyumin Whang; Trinuch Eiampongpaiboon; University of Washington, Seattle; Peking University; Mahidol University; University of Texas at San Antonio; University of Texas School of Dentistry; CAO Group, Inc.
    Copyright©American Journal of Dentistry. PURPOSE: The study and development of antibacterial materials for use in dental applications is growing with the development of novel materials and procedures. Examination of the effects of such antibacterial materials on oral pathogens as well as on stability and longevity of dental restorations is of paramount importance to the field. RESULTS: This review addressed the range of topics covered by the manuscripts presented at the Seoul symposium on antibacterial dental materials. CLINICAL SIGNIFICANCE: Based on the presented works, it seems that the emerging antibacterial and bioactive mate-rials can potentially benefit restorative dentistry; however, like many other subjects in clinical dentistry, good quality evidence on their effectiveness under clinical situations is yet to be accumulated.
  • No Thumbnail Available
    PublicationMetadata only
    Surface roughness resulting from wear of lithia-disilicate-based posterior crowns
    (2010-06-01) Kallaya Suputtamongkol; Amornrat Wonglamsam; Trinuch Eiampongpaiboon; Sumi Malla; Kenneth J. Anusavice; Mahidol University; University of Florida College of Dentistry
    The objective of this study was to determine the surface roughness that occurred as a result of wear of all-ceramic crowns after 2 years of intraoral service. The ceramic material used in this study was a lithia-disilicate-based all-ceramic core ceramic and a glass-phase veneer ceramic. Posterior bilayer crowns were made for 30 subjects, who were recalled annually. At each recall time, the quality of crowns and adjacent gingival tissues were examined for acceptability, and impressions were made for replica models. The occlusal contacts of each ceramic crown were identified and surface roughness (Ra) measurement was performed on the replica model using a contact profilometer. Mean surface roughness values were analyzed using a repeated measure ANOVA. The wear patterns of contact surfaces were also characterized using a scanning electron microscope. From 30 ceramic crowns, 12 premolars and 13 molars were used for surface roughness measurements. For molar crowns, the surface roughness (Ra) at baseline was 1.76±0.43μm and the roughness significantly increased after 1 year and 2 years (p<0.05). For premolar crowns, the increase in roughness values was significantly different only after 2 years from 1.49±0.22 to 1.9±0.44μm (p<0.05). Roughening of ceramic surfaces was observed over the entire occlusal area, especially in the contact zones. Loss of superficial ceramic material as a result of microfracture was the reason for surface roughening. In conclusion, the surface roughness of ceramic crowns was significantly increased after 2 years. The increase in surface roughness indicated the degradation of the ceramic crown surfaces over time that resulted from the wear process. © 2010 Elsevier B.V.