Process-intensified phosphate capture using lanthanum-functionalized PVA/chitosan hydrogel in a continuous-flow microscale-based device
item.page.dc.date.issued
2026-11-01
item.page.dc.type
item.page.dc.identifier.issn
02552701
item.page.dc.identifier.doi
item.page.dc.identifier.scopus
2-s2.0-105049148110
item.page.oaire.citation.title
Chemical Engineering and Processing Process Intensification
item.page.oaire.citation.volume
229
item.page.dc.rights.holder
SCOPUS
item.page.dc.identifier.citation
Chemical Engineering and Processing Process Intensification Vol.229 (2026)
punsarn.item.page.citation
Pantakitcharoenkul J., chompumuangchuen K., Naruphontjirakul P., Coblyn M., Jovanovic G. Process-intensified phosphate capture using lanthanum-functionalized PVA/chitosan hydrogel in a continuous-flow microscale-based device. Chemical Engineering and Processing Process Intensification Vol.229 (2026). doi:10.1016/j.cep.2026.111033 Retrieved from: https://repository.li.mahidol.ac.th/handle/123456789/118838
item.page.dc.title
Process-intensified phosphate capture using lanthanum-functionalized PVA/chitosan hydrogel in a continuous-flow microscale-based device
item.page.dc.contributor.author
item.page.oairecerif.author.affiliation
item.page.dc.contributor.correspondence
item.page.dc.contributor.other
item.page.dc.description.abstract
Managing hyperphosphatemia in chronic kidney disease (CKD) and tumor lysis syndrome (TLS) remains challenging due to the kinetic mismatch between rapid dialytic extraction and slow intracellular phosphate mobilization. This study presents the fabrication, characterization, and computational optimization of a lanthanum-doped poly(vinyl alcohol)/chitosan (PVA/CS 315-La) hydrogel film in a microscale continuous-flow device for phosphate capture. Lanthanum-bearing nanoparticles transformed the hydrogel from an isotropic sponge to a dense, aligned fibrous architecture dose-dependently. Characterization indicated lanthanum entrapment without disrupting the network. In dynamic in vitro flow, the lanthanum-functionalized hydrogel (PVA/CS 315-La5) achieved 42.9% phosphate removal (1.47 to 0.84 ± 0.12 mM). Response Surface Methodology (RSM) mapped the coupled effects of flow rate, active site density (S<inf>ads</inf>), and intra-gel diffusivity (D<inf>i,gel</inf>) on phosphate depletion time. The validated quadratic model (R² = 0.9957) identified an optimal configuration of 6.05 mL/min flow rate and S<inf>ads</inf> of 962.6 mol/m³ as the mathematical optimum for 36-h depletion; however, long-duration sensitivity analysis identified a narrower practical window of S<inf>ads</inf> ≈ 150–200 mol/m³ at the same flow rate as favorable for a gradual, monotonic clearance profile, avoiding the early quasi-burst extraction observed at higher loadings. These findings establish an integrated framework linking sorbent chemistry, device hydrodynamics, and computational optimization for designing continuous sorbent-based phosphate capture devices.