Defect-engineered biphasic calcium phosphate scaffolds from Nile tilapia bone: Calcination-controlled phase evolution and structure–bioactivity coupling
3
item.page.dc.date.issued
2026-08-01
item.page.dc.type
item.page.dc.identifier.issn
02641275
item.page.dc.identifier.eissn
18734197
item.page.dc.identifier.doi
item.page.dc.identifier.scopus
2-s2.0-105050457976
item.page.oaire.citation.title
Materials and Design
item.page.oaire.citation.volume
268
item.page.dc.rights.holder
SCOPUS
item.page.dc.identifier.citation
Materials and Design Vol.268 (2026)
punsarn.item.page.citation
Wannasen L., Pimsawat A., Mingmuang Y., Khamkhantee N., Daengsakul S., Wongprasod S., Tanapongpisit N., Rojviriya C., Vongpramate D., Saenrang W., Wongrakpanich A., Khamkongkaeo A. Defect-engineered biphasic calcium phosphate scaffolds from Nile tilapia bone: Calcination-controlled phase evolution and structure–bioactivity coupling. Materials and Design Vol.268 (2026). doi:10.1016/j.matdes.2026.116429 Retrieved from: https://repository.li.mahidol.ac.th/handle/123456789/119099
item.page.dc.title
Defect-engineered biphasic calcium phosphate scaffolds from Nile tilapia bone: Calcination-controlled phase evolution and structure–bioactivity coupling
item.page.dc.contributor.author
item.page.dc.contributor.correspondence
item.page.dc.contributor.other
item.page.dc.description.abstract
Porous biphasic calcium phosphate (BCP) scaffolds were fabricated from Nile tilapia bone waste via microwave-assisted processing. The extracted powders were subsequently calcined at 500–1000 °C to tailor precursor characteristics, phase evolution, and defect chemistry. Increasing calcination temperature promoted particle coarsening and carbonate removal. Below 700 °C, single-phase hydroxyapatite (HAp) was retained. At ≥ 700 °C, HAp/β-tricalcium phosphate (β-TCP) compositions emerged, with β-TCP content increasing from 7.6 % to 16.9 %. Scaffolds fabricated via polyurethane sponge replication and sintered at 1250 °C exhibited highly interconnected porous architectures with porosities ranging from 77.5 % to 89 %. Carbonate-rich precursors promoted shrinkage, microcracking, and finer pore fractions, whereas higher-temperature calcined powders yielded crack-free scaffolds with improved structural stability. Sintering further increased β-TCP content (15–24.4 %) and promoted dehydroxylation, as confirmed by Fourier Transform Infrared Spectroscopy (FTIR) and X-ray photoelectron spectroscopy (XPS), indicating the formation of OH<sup>−</sup> vacancies. In vitro evaluation revealed that scaffolds calcined at 500 °C exhibited the highest direct cell proliferation due to a favorable micropore fraction, while those calcined at 1000 °C demonstrated superior bioactivity attributed to the greatest OH<sup>−</sup> vacancy concentration (ΔOH<sup>−</sup> = 10.77 %). These findings establish calcination temperature as a critical processing parameter governing phase evolution, defect chemistry, and biological performance in sustainable biowaste-derived BCP scaffolds.