Publication:
Properties of peroxide cured highly purified natural rubber

dc.contributor.authorA. Nimpaiboonen_US
dc.contributor.authorJ. Sakdapipanichen_US
dc.contributor.otherMahidol Universityen_US
dc.date.accessioned2018-06-11T04:48:00Z
dc.date.available2018-06-11T04:48:00Z
dc.date.issued2012-10-01en_US
dc.description.abstractHighly purified natural rubbers (HPNR) were prepared by saponification of fresh latex (FL-latex) in the presence of surfactant. It was found that nitrogen content markedly decreased from 0.86% to 0.1% after the process. Nitrosamine free vulcanized rubber could be prepared by peroxide curing system to give a same level of physical properties as those of deproteinized NR, STR 5L rubber and synthetic isoprene rubber (IR). The tensile strength obtained was about 12 MPa. The color after vulcanization was light-yellowish. Owing to the low protein allergens, nitrosamine free, and good physical properties, HPNR vulcanized by peroxide system is an attractive material for medical application.en_US
dc.identifier.citationKGK Kautschuk Gummi Kunststoffe. Vol.65, No.10 (2012), 55-59en_US
dc.identifier.issn09483276en_US
dc.identifier.other2-s2.0-84867513983en_US
dc.identifier.urihttps://repository.li.mahidol.ac.th/handle/20.500.14594/14143
dc.rightsMahidol Universityen_US
dc.rights.holderSCOPUSen_US
dc.source.urihttps://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84867513983&origin=inwarden_US
dc.subjectEngineeringen_US
dc.subjectMaterials Scienceen_US
dc.titleProperties of peroxide cured highly purified natural rubberen_US
dc.typeArticleen_US
dspace.entity.typePublication
mu.datasource.scopushttps://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84867513983&origin=inwarden_US