Publication: Effect of thermocycling on the durability of etch-and-rinse and self-etch adhesives on dentin
| dc.contributor.author | Ketkamon Sangwichit | en_US |
| dc.contributor.author | Ruksaphon Kingkaew | en_US |
| dc.contributor.author | Pong Pongprueksa | en_US |
| dc.contributor.author | Pisol Senawongse | en_US |
| dc.contributor.other | Mahidol University | en_US |
| dc.date.accessioned | 2018-12-11T02:43:09Z | |
| dc.date.accessioned | 2019-03-14T08:04:40Z | |
| dc.date.available | 2018-12-11T02:43:09Z | |
| dc.date.available | 2019-03-14T08:04:40Z | |
| dc.date.issued | 2016-01-01 | en_US |
| dc.description.abstract | © 2016, Japanese Society for Dental Materials and Devices. All rights reserved. The objective was to compare bond strengths of adhesives with/without thermocycling and to analyze the micromorphology of resindentin interfaces. Flat dentin surfaces were prepared and divided into eight groups to bond with four etch-and-rinse adhesives (Optibond FL, Adper Scotchbond Multi-Purpose, Optibond Solo Plus, and Single Bond 2) and four self-etch adhesives (Clearfil SE Bond, Adper SE Plus, Clearfil S3 Bond and Adper Easy Bond). Specimens were further divided into two subgroups subjected for with/without thermocycling and then subjected to both micro-tensile test and resin-dentin interface evaluation. The results revealed that there were significant differences in bond strength between the groups with and without thermocycling for all etch-and-rinse groups and for the Adper Easy Bond self-etch group (p<0.01). Clearfil SE Bond demonstrated highly durable bond strengths. Furthermore, more silver ion uptake was observed at the resin-dentin interfaces for all etch-and-rinse adhesives and Adper SE Plus and Adper Easy Bond after thermocycling. | en_US |
| dc.identifier.citation | Dental Materials Journal. Vol.35, No.3 (2016), 360-368 | en_US |
| dc.identifier.doi | 10.4012/dmj.2015-253 | en_US |
| dc.identifier.issn | 18811361 | en_US |
| dc.identifier.issn | 02874547 | en_US |
| dc.identifier.other | 2-s2.0-84971443033 | en_US |
| dc.identifier.uri | https://repository.li.mahidol.ac.th/handle/123456789/43614 | |
| dc.rights | Mahidol University | en_US |
| dc.rights.holder | SCOPUS | en_US |
| dc.source.uri | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84971443033&origin=inward | en_US |
| dc.subject | Dentistry | en_US |
| dc.subject | Materials Science | en_US |
| dc.title | Effect of thermocycling on the durability of etch-and-rinse and self-etch adhesives on dentin | en_US |
| dc.type | Article | en_US |
| dspace.entity.type | Publication | |
| mu.datasource.scopus | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84971443033&origin=inward | en_US |