Publication:
Influence of styrene on grafting efficiency of maleic anhydride onto natural rubber

dc.contributor.authorJ. Saelaoen_US
dc.contributor.authorP. Phinyocheepen_US
dc.contributor.otherMahidol Universityen_US
dc.date.accessioned2018-06-21T08:12:39Z
dc.date.available2018-06-21T08:12:39Z
dc.date.issued2005-01-05en_US
dc.description.abstractGrafting of maleic anhydride (MA) onto natural rubber (NR) has been investigated by using a radical initiated grafting process. NR was masticated to lower molecular weight than the original NR before treatment with 0.5-1.5% by mole of benzoyl peroxide (BPO) and 5-25% by mole of MA in toluene solution. Fourier transform infrared spectroscopy (FTIR) and titration method were used to analyze the fixation of MA on the NR. The reaction temperature was varied from 60 to 80°C. The % grafting of MA was higher at higher temperatures. Compared to the reaction without styrene, the addition of 0.1% by mole of styrene in the grafting process increased % MA grafting up to two times. It is postulated that the styrene may act as a charge transfer complex for the reaction of NR with MA. © 2004 Wiley Periodicals, Inc.en_US
dc.identifier.citationJournal of Applied Polymer Science. Vol.95, No.1 (2005), 28-38en_US
dc.identifier.doi10.1002/app.20810en_US
dc.identifier.issn00218995en_US
dc.identifier.other2-s2.0-10844264382en_US
dc.identifier.urihttps://repository.li.mahidol.ac.th/handle/123456789/16456
dc.rightsMahidol Universityen_US
dc.rights.holderSCOPUSen_US
dc.source.urihttps://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=10844264382&origin=inwarden_US
dc.subjectChemistryen_US
dc.subjectMaterials Scienceen_US
dc.titleInfluence of styrene on grafting efficiency of maleic anhydride onto natural rubberen_US