Publication:
Effect of epoxidation and surface modification on backing-required properties of peroxide prevulcanized natural rubber-based films

dc.contributor.authorSupa Wirasateen_US
dc.contributor.authorChompoonuch Chokbunpiamen_US
dc.contributor.authorRattaporn Thonggoomen_US
dc.contributor.authorPramuan Tangboriboonraten_US
dc.contributor.otherMahidol Universityen_US
dc.date.accessioned2018-11-09T02:28:50Z
dc.date.available2018-11-09T02:28:50Z
dc.date.issued2014-03-01en_US
dc.description.abstractThe effect of epoxidation and surface modification by acrylamide grafting on backing-required properties of peroxide prevulcanized natural rubber (PPNR)-based films was investigated. Backing-required properties including oxygen transmission rate (OTR), water vapor transmission rate (WVTR) and Young's modulus were determined. In situ epoxidation of natural rubber (NR) latex was carried out using hydrogen peroxide/formic acid system. Both NR and epoxidized natural rubber (ENR) latexes were prevulcanized by tert-butyl hydroperoxide/fructose system before film casting. In the case of surface modification, acrylamide was grafted on PPNR surface by dipping the PPNR strip treated with O2 plasma into an aqueous solution of acrylamide monomer (AAm). Epoxidation showed more pronounced effect on the backing-required properties than surface grafting. As mole percentage epoxide increased, OTR decreased by 22-35%, whereas WVTR and Young's modulus increased by 116-170% and 56-138%, respectively, depending on mole percentage epoxide. In the case of surface grafting, it was found that all OTR, WVTR and Young's modulus were slightly higher than those of unmodified films. © The Author(s) 2012.en_US
dc.identifier.citationJournal of Elastomers and Plastics. Vol.46, No.2 (2014), 156-174en_US
dc.identifier.doi10.1177/0095244312465297en_US
dc.identifier.issn15308006en_US
dc.identifier.issn00952443en_US
dc.identifier.other2-s2.0-84893109492en_US
dc.identifier.urihttps://repository.li.mahidol.ac.th/handle/20.500.14594/34115
dc.rightsMahidol Universityen_US
dc.rights.holderSCOPUSen_US
dc.source.urihttps://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84893109492&origin=inwarden_US
dc.subjectMaterials Scienceen_US
dc.titleEffect of epoxidation and surface modification on backing-required properties of peroxide prevulcanized natural rubber-based filmsen_US
dc.typeArticleen_US