Publication: Preparation of Ni/MgOZrO<inf>2</inf>nanocrystals by citrate sol-gel method
dc.contributor.author | Wimonrat Trakarnpruk | en_US |
dc.contributor.author | Charnsak Sukkaew | en_US |
dc.contributor.other | Mahidol University | en_US |
dc.date.accessioned | 2018-07-12T02:26:31Z | |
dc.date.available | 2018-07-12T02:26:31Z | |
dc.date.issued | 2008-07-28 | en_US |
dc.description.abstract | Ni/MgOZrO2nanocrystals were prepared by the citrate sol-gel method and characterized by X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, scanning electron microscopy (SEM) and nitrogen adsorption methods. Results show that the powders prepared by calcination for 4 h at a temperature of 800 °C have a particle size of 15 nm and possess a surface area of 145 m2/g. © 2007 Elsevier B.V. All rights reserved. | en_US |
dc.identifier.citation | Journal of Alloys and Compounds. Vol.460, No.1-2 (2008), 565-569 | en_US |
dc.identifier.doi | 10.1016/j.jallcom.2007.06.018 | en_US |
dc.identifier.issn | 09258388 | en_US |
dc.identifier.other | 2-s2.0-44449133562 | en_US |
dc.identifier.uri | https://repository.li.mahidol.ac.th/handle/20.500.14594/19211 | |
dc.rights | Mahidol University | en_US |
dc.rights.holder | SCOPUS | en_US |
dc.source.uri | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=44449133562&origin=inward | en_US |
dc.subject | Engineering | en_US |
dc.subject | Materials Science | en_US |
dc.title | Preparation of Ni/MgOZrO<inf>2</inf>nanocrystals by citrate sol-gel method | en_US |
dc.type | Article | en_US |
dspace.entity.type | Publication | |
mu.datasource.scopus | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=44449133562&origin=inward | en_US |