Publication: Structural characterization of highly cis-1,4-polybutadiene: A comparing study in swollen and solid state using NMR technique
dc.contributor.author | Jitladda Sakdapipanich | en_US |
dc.contributor.author | Tippawan Kowitteerawut | en_US |
dc.contributor.author | Kawahara Seiichi | en_US |
dc.contributor.author | Yasuyuki Tanaka | en_US |
dc.contributor.other | Mahidol University | en_US |
dc.contributor.other | Nagaoka University of Technology | en_US |
dc.date.accessioned | 2018-09-07T09:39:33Z | |
dc.date.available | 2018-09-07T09:39:33Z | |
dc.date.issued | 2001-08-31 | en_US |
dc.description.abstract | Commercial highly cis-1,4-polybutadiene was cured out by benzoyl peroxide from 3 to 12 phr in toluene solution. The structural characterization of resulting gel fraction or cured rubber was carried out in both swollen- and solid-state 13C-NMR measurements. The assignment of observed chemical shift proposed by using a shift factor method and empirical calculation using HOSE method. | en_US |
dc.identifier.citation | Polymer Bulletin. Vol.46, No.6 (2001), 479-485 | en_US |
dc.identifier.doi | 10.1007/s002890170035 | en_US |
dc.identifier.issn | 01700839 | en_US |
dc.identifier.other | 2-s2.0-0034886830 | en_US |
dc.identifier.uri | https://repository.li.mahidol.ac.th/handle/123456789/26504 | |
dc.rights | Mahidol University | en_US |
dc.rights.holder | SCOPUS | en_US |
dc.source.uri | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=0034886830&origin=inward | en_US |
dc.subject | Chemistry | en_US |
dc.subject | Materials Science | en_US |
dc.subject | Physics and Astronomy | en_US |
dc.title | Structural characterization of highly cis-1,4-polybutadiene: A comparing study in swollen and solid state using NMR technique | en_US |
dc.type | Article | en_US |
dspace.entity.type | Publication | |
mu.datasource.scopus | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=0034886830&origin=inward | en_US |