Publication: Raman spectroscopic study of non-catalytic hydrogenation of unsaturated rubbers
dc.contributor.author | Jareerat Samran | en_US |
dc.contributor.author | Pranee Phinyocheep | en_US |
dc.contributor.author | Philippe Daniel | en_US |
dc.contributor.author | Daniel Derouet | en_US |
dc.contributor.author | Jean Yves Buzaré | en_US |
dc.contributor.other | Mahidol University | en_US |
dc.contributor.other | Universite du Maine Le Mans - Laval | en_US |
dc.date.accessioned | 2018-07-24T03:39:42Z | |
dc.date.available | 2018-07-24T03:39:42Z | |
dc.date.issued | 2004-12-01 | en_US |
dc.description.abstract | The non-catalytic hydrogenation of natural rubber (NR) and two epoxidized NRs (ENRs) i.e. ENR-22 and ENR-40 containing 22 and 40 mol% of epoxide, respectively, was carried out using p-toluenesulfonylhydrazide (TSH) as a hydrogenating agent. A two-fold molar excess of TSH compared with unsaturated units of the rubber was used. The evidence of hydrogenation is a decrease in the intensity of the characteristic signal of the carbon-carbon double bond stretching vibration of the rubber in both the Raman and FT-IR spectra. The percentage hydrogenation was successfully determined by Raman spectroscopy since the vibrational mode of the carbon-carbon unsaturation is strongly Raman active. The progress of the hydrogenation could be monitored by means of the techniques mentioned above as a function of reaction time. The maximum degree of hydrogenation of NR is ∼89% whereas in the case of ENR-22 and ENR-40 it reaches 94 and 96%, respectively. Solid-state 13C NMR spectroscopy was also used to confirm the microstructure characteristics of the hydrogenated rubbers. 13C NMR analysis showed that cis-trans isomerization of carbon-carbon unsaturations occur during hydrogenation. Copyright © 2004 John Wiley & Sons, Ltd. | en_US |
dc.identifier.citation | Journal of Raman Spectroscopy. Vol.35, No.12 (2004), 1073-1080 | en_US |
dc.identifier.doi | 10.1002/jrs.1256 | en_US |
dc.identifier.issn | 03770486 | en_US |
dc.identifier.other | 2-s2.0-11244288315 | en_US |
dc.identifier.uri | https://repository.li.mahidol.ac.th/handle/20.500.14594/21267 | |
dc.rights | Mahidol University | en_US |
dc.rights.holder | SCOPUS | en_US |
dc.source.uri | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=11244288315&origin=inward | en_US |
dc.subject | Chemistry | en_US |
dc.subject | Materials Science | en_US |
dc.title | Raman spectroscopic study of non-catalytic hydrogenation of unsaturated rubbers | en_US |
dc.type | Article | en_US |
dspace.entity.type | Publication | |
mu.datasource.scopus | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=11244288315&origin=inward | en_US |