Toward a Circular Bioeconomy: Exploring Pineapple Stem Starch Film as a Plastic Substitute in Single Use Applications
7
item.page.dc.date.issued
2023-05-01
item.page.dc.type
item.page.dc.identifier.eissn
20770375
item.page.dc.identifier.doi
item.page.dc.identifier.scopus
2-s2.0-85160212441
item.page.oaire.citation.title
Membranes
item.page.oaire.citation.volume
13
item.page.oaire.citation.issue
5
item.page.dc.rights.holder
SCOPUS
item.page.dc.identifier.citation
Membranes Vol.13 No.5 (2023)
punsarn.item.page.citation
Namphonsane A., Suwannachat P., Chia C.H., Wongsagonsup R., Smith S.M., Amornsakchai T. Toward a Circular Bioeconomy: Exploring Pineapple Stem Starch Film as a Plastic Substitute in Single Use Applications. Membranes Vol.13 No.5 (2023). doi:10.3390/membranes13050458 Retrieved from: https://repository.li.mahidol.ac.th/handle/123456789/82936
item.page.dc.title
Toward a Circular Bioeconomy: Exploring Pineapple Stem Starch Film as a Plastic Substitute in Single Use Applications
item.page.dc.contributor.author
item.page.oairecerif.author.affiliation
item.page.dc.contributor.other
item.page.dc.description.abstract
In this study, biodegradable starch film was developed from pineapple stem waste as a substitute for non-biodegradable petroleum-based films for single-use applications where strength is not too demanding. High amylose starch from a pineapple stem was used as the matrix. Glycerol and citric acid were used as additives to adjust the ductility of the material. Glycerol content was fixed at 25% while that of citric acid varied from 0 to 15% by weight of starch. Films with a wide range of mechanical properties can be prepared. As more citric acid is added, the film becomes softer and weaker, and has greater elongation at the break. Properties range from a strength of about 21.5 MPa and 2.9% elongation to a strength of about 6.8 MPa and 35.7% elongation. An X-ray diffraction study showed that the films were semi-crystalline. The films were also found to be water-resistant and can be heat-sealed. An example of a single-use package was demonstrated. A soil burial test confirmed that the material was biodegradable and completely disintegrated into sizes smaller than 1 mm within one month.