Publication: Shear bond strength between autopolymerizing acrylic resin and Co-Cr alloy using different primers
Issued Date
2012-10-30
Resource Type
ISSN
18811361
02874547
02874547
Other identifier(s)
2-s2.0-84867891914
Rights
Mahidol University
Rights Holder(s)
SCOPUS
Bibliographic Citation
Dental Materials Journal. Vol.31, No.5 (2012), 765-771
Suggested Citation
Sasiwimol Sanohkan, Somchai Urapepon, Choltacha Harnirattisai, Chakrit Sirisinha, Panya Sunintaboon Shear bond strength between autopolymerizing acrylic resin and Co-Cr alloy using different primers. Dental Materials Journal. Vol.31, No.5 (2012), 765-771. doi:10.4012/dmj.2012-051 Retrieved from: https://repository.li.mahidol.ac.th/handle/20.500.14594/14071
Research Projects
Organizational Units
Authors
Journal Issue
Thesis
Title
Shear bond strength between autopolymerizing acrylic resin and Co-Cr alloy using different primers
Other Contributor(s)
Abstract
This study aimed to examine the shear bond strength between cobalt chromium alloy and autopolymerizing acrylic resin using experimental primers containing 5, 10, and 15 wt% of 4-methacryloxyethyl trimellitic anhydride or 1, 2, and 3 wt% of 3-methacryloxypropyl-trimethoxysilane comparison to 5 commercial primers (ML primers, Alloy primer, Metal/Zirconia primer, Monobond S, and Monobond plus). Sixty alloy specimens were sandblasted and treated with each primer before bonded with an acrylic resin. The control group was not primed. The shear bond strengths were tested and statistically compared. Specimens treated with commercial primers significantly increased the shear bond strength of acrylic resin to cobalt chromium alloy (p < 0.05). The highest shear bond strength was found in the Alloy primer group. Among experimental group, using 10 wt% of 4-methacryloxyethyl trimellitic anhydride -or 2 wt% of 3-methacryloxypropyltrimethoxysilane enhanced highest shear bond strength. The experimental and commercial primers in this study all improved bonding of acrylic resin to cobalt chromium alloy.